Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   Hungary. Structural steel    

Equivalents to grade BC2

    Country   -   Hungary         Standard   -   MSZ 31         Grade   -   BC2    

    20KH   ( 20Х )   -   Alloy structurall steel

  20KH   ( 20Х ),      



20KH   ( 20Х )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 20KH   ( 20Х )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them
В71 - Low-carbon steel wire


BC2 Hungary Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.