Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   Japan. Structural steel    

Equivalents to grade S45C

    Country   -   Japan         Standard   -   JIS G4051         Grade   -   S45C    

NEW !  
SteelJIS : Free database of Japanese steels and alloys
SteelJIS.com contains the information about chemical composition and properties
more than 1400 Japanese engineering materials.
  SteelJIS.com:   Japanese Steels and Alloys



    45   ( 45 )   -   High quality structural carbon steel
    45G   ( 45Г )   -   Alloy structurall steel

  45   ( 45 ),         45G   ( 45Г ),      



45   ( 45 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 45   ( 45 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
В71 - Low-carbon steel wire
В72 - Medium-high and high-carbon steel wire
B76 - Metal nets

45G   ( 45Г )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 45G   ( 45Г )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
В71 - Low-carbon steel wire


S45C Japan Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.