Characteristics for grade     15Kh6SYu   ( 15Х6СЮ )



      Grade :   15Kh6SYu   ( 15Х6СЮ ) (   Х6СЮ     ЭИ428   )
      Classification :   Low alloy high-temperature steel
      Equivalent grades:   Go here



Chemical composition in % for grade   15Kh6SYu   ( 15Х6СЮ )
C Si Mn S P CrAl
max   0.151.2 - 1.8max   0.5max   0.025max   0.035.5 - 70.7 - 1.1


Mechanical properties under Т=20oС for grade   15Kh6SYu   ( 15Х6СЮ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75     440 245 20 40 Annealing 750 - 800oC,Cooling air,


Equivalent steels for grade     15Kh6SYu   ( 15Х6СЮ )
Warning! Indicated both exact and nearest equivalents.
GermanyFranceEuropeanItalyCzechia
DIN,WNrAFNOREN UNICSN
1.4713
X10CrAlSi7
Z8CA7
1.4713
X10CrAlSi7
X7AL
17113



Types of delivery of grade   15Kh6SYu   ( 15Х6СЮ )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  15Kh6SYu   ( 15Х6СЮ ) - Low alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru