Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Stainless steel

Characteristics for grade     09KH15N8YU   ( 09Х15Н8Ю )



      Grade :   09KH15N8YU   ( 09Х15Н8Ю ) (   Х15Н9Ю     ЭИ904     09Х15Н8Ю1   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:     Is absent



Chemical composition in % for grade   09KH15N8YU   ( 09Х15Н8Ю )
C Si Mn Ni S P CrAl
max   0.09max   0.8max   0.87 - 9.4max   0.025max   0.03514 - 160.7 - 1.3


Mechanical properties under Т=20oС for grade   09KH15N8YU   ( 09Х15Н8Ю )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet thin, GOST 4986-79     1130   8-15  Normalizing 1030 - 1070oC,
Sheet thin, GOST 5582-75     1080   20   Normalizing 1040 - 1080oC,
Sheet thin cold-worked , GOST 4986-79     1270   2-4   
Sheet thin, GOST 4986-79     980   3-6   



Types of delivery of grade   09KH15N8YU   ( 09Х15Н8Ю )
B23 - Sheets and Strips
B33 - Sheets and Strips
B34 - Ribbons


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  09KH15N8YU   ( 09Х15Н8Ю ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys