Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   High-temperature or heat-resistant steel and alloy

Characteristics for grade     KhN65VMTYu   ( ХН65ВМТЮ )



      Grade :   KhN65VMTYu   ( ХН65ВМТЮ ) (   ХН65МВТЮ     ЭИ893     ХН65ВМТЮ-ВД     ЭИ893-ВД     ХН65ВМТЮ-ВИ     ЭИ893-ВИ   )
      Classification :   Hidh-temperature or heat-resistant alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   KhN65VMTYu   ( ХН65ВМТЮ )
Fe C Si Mn Ni S P Cr Ce Mo W TiAl B
max   3max   0.07max   0.6max   0.660.968 - 70.6max   0.012max   0.01515 - 17max   0.0253.5 - 4.58.5 - 101.2 - 1.61.2 - 1.6max   0.01
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   KhN65VMTYu   ( ХН65ВМТЮ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 23705-79   longitudinal 830 490 20 25580 


Technological properties for grade   KhN65VMTYu   ( ХН65ВМТЮ )
  Weldability: hard weldability.


Physical properties for grade   KhN65VMTYu   ( ХН65ВМТЮ )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.22   12.7 8800    
100 2.14 11.5        
200 2.1   13      
300 2.02 12.3 13.8      
400 1.95 12.75 15.5      
500 1.9 13 17.2      
600 1.84 13.2 19.7      
700 1.74 14 23.6      
800 1.65 14.3 27.2      
900 1.6 15        
T E 10- 5 a 10 6 l r C R 10 9



Types of delivery of grade   KhN65VMTYu   ( ХН65ВМТЮ )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  KhN65VMTYu   ( ХН65ВМТЮ ) - Hidh-temperature or heat-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.