Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Stainless steel

Characteristics for grade     03KHN28MDT   ( 03ХН28МДТ )



      Grade :   03KHN28MDT   ( 03ХН28МДТ ) (   000Х23Н28М3Д3Т     ЭП516   )
      Classification :   Corrosion-resistant alloy
      Equivalent grades:   Go here



Chemical composition in % for grade   03KHN28MDT   ( 03ХН28МДТ )
Fe C Si Mn Ni S P Cr Mo Ti Cu
36.915 - 46.5max   0.03max   0.8max   0.826 - 29max   0.02max   0.03522 - 252.5 - 30.5 - 0.92.5 - 3.5


Mechanical properties under Т=20oС for grade   03KHN28MDT   ( 03ХН28МДТ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet trick, GOST 7350-77     540 215 35   Guenching 1040 - 1080oC,Cooling water,


Equivalent steels for grade     03KHN28MDT   ( 03ХН28МДТ )
Warning! Indicated both exact and nearest equivalents.
Germany
DIN,WNr
X3NiCrCuMoTi2730



Types of delivery of grade   03KHN28MDT   ( 03ХН28МДТ )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  03KHN28MDT   ( 03ХН28МДТ ) - Corrosion-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru