Characteristics for grade     08KH17N5M3   ( 08Х17Н5М3 )



      Grade :   08KH17N5M3   ( 08Х17Н5М3 ) (   Х17Н5М3     ЭИ925   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   08KH17N5M3   ( 08Х17Н5М3 )
C Si Mn Ni S P Cr Mo
0.06 - 0.1max   0.8max   0.84.5 - 5.5max   0.02max   0.03516 - 17.53 - 3.5


Mechanical properties under Т=20oС for grade   08KH17N5M3   ( 08Х17Н5М3 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Forging, GOST 25054-81     1176 833 10-1535-40390-690 
Sheet thin, GOST 4986-79     1130   8-16  Normalizing
Sheet thin, GOST 5582-75     1180 610 20   Guenching 1030 - 1080oC, air,
Sheet thin cold-worked , GOST 4986-79     1230   2-4   


    Brinell hardness for     08KH17N5M3   ( 08Х17Н5М3 )   ,     Forging GOST 25054-81 HB 10 -1 = 341 - 415   MPa


Technological properties for grade   08KH17N5M3   ( 08Х17Н5М3 )
  Weldability: without limitations.


Equivalent steels for grade     08KH17N5M3   ( 08Х17Н5М3 )
Warning! Indicated both exact and nearest equivalents.
USAGermany
-DIN,WNr
AM350
X4CrNiMo16-5



Types of delivery of grade   08KH17N5M3   ( 08Х17Н5М3 )
B03 - Metal forming treatment. Forgings
B23 - Sheets and Strips
B33 - Sheets and Strips
B34 - Ribbons


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  08KH17N5M3   ( 08Х17Н5М3 ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru