Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Stainless steel

Characteristics for grade     09KH17N7YU   ( 09Х17Н7Ю )



      Grade :   09KH17N7YU   ( 09Х17Н7Ю ) (   0Х17Н7Ю   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   09KH17N7YU   ( 09Х17Н7Ю )
C Si Mn Ni S P CrAl
max   0.09max   0.8max   0.087 - 8max   0.02max   0.0316 - 17.50.5 - 0.8


Mechanical properties under Т=20oС for grade   09KH17N7YU   ( 09Х17Н7Ю )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet trick, GOST 7350-77     830 735 12  490Guenching and drawing


Equivalent steels for grade     09KH17N7YU   ( 09Х17Н7Ю )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanChinaSweden
-DIN,WNrJIS AFNORBSEN GBSS
631
S17700
1.4568
X7CrNiAl17-7
SUS631
Z8CNA17-7
Z9CNA17-07
301S81
1.4568
X7CrNiAl17-7
0Cr17Ni7Al
2388



Types of delivery of grade   09KH17N7YU   ( 09Х17Н7Ю )
B23 - Sheets and Strips
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  09KH17N7YU   ( 09Х17Н7Ю ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru