Characteristics for grade     13KHNDFTL   ( 13ХНДФТЛ )

      Grade :     13KHNDFTL   ( 13ХНДФТЛ )
      Classification :   Casting alloy steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   13KHNDFTL   ( 13ХНДФТЛ )
C Si Mn Ni S P Cr V Ti Cu
max   0.160.2 - 0.40.4 - 0.91.2 - 1.6max   0.03max   0.030.15 - 0.40.06 - 0.120.04 - 0.10.65 - 0.9


Mechanical properties under Т=20oС for grade   13KHNDFTL   ( 13ХНДФТЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     491 392 18 30491 


Heat treatment of the material   13KHNDFTL   ( 13ХНДФТЛ )
Normalizing 950 - 970 ° C, or Normalizing 900 - 920 ° C, Tempering 530 - 560 ° C


Equivalent steels for grade     13KHNDFTL   ( 13ХНДФТЛ )
Warning! Indicated both exact and nearest equivalents.
Bulgaria
BDS
13ChNDFTL

Types of delivery of grade   13KHNDFTL   ( 13ХНДФТЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  13KHNDFTL   ( 13ХНДФТЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru