Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Casting steel

Characteristics for grade     12KH18N12BL   ( 12Х18Н12БЛ )



      Grade :     12KH18N12BL   ( 12Х18Н12БЛ )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:     Is absent



Chemical composition in % for grade   12KH18N12BL   ( 12Х18Н12БЛ )
C Si Mn Ni S P Cr Nb
max   0.12max   0.550.5 - 111 - 13max   0.025max   0.0217 - 190.7 - 1.1


Mechanical properties under Т=20oС for grade   12KH18N12BL   ( 12Х18Н12БЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     392 196 13 18196Guenching 1180oC,Cooling air, Ageing 800oC, 10h,Ageing 750oC, 16h,


Heat treatment of the material   12KH18N12BL   ( 12Х18Н12БЛ )
Hardening 1170 - 1190 ° C, Air cooling. Aging 790 - 810 ° C, 10 hours , Aging 740 - 760 ° C, 16 hours ,



Types of delivery of grade   12KH18N12BL   ( 12Х18Н12БЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  12KH18N12BL   ( 12Х18Н12БЛ ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru