Characteristics for grade     St6ps   ( Ст6пс )



      Grade :     St6ps   ( Ст6пс )
      Classification :   Normal quality structural carbon steel
      Equivalent grades:   Go here



Chemical composition in % for grade   St6ps   ( Ст6пс )
C Si Mn Ni S P Cr N Cu As
0.38 - 0.490.05 - 0.150.5 - 0.8max   0.3max   0.05max   0.04max   0.3max   0.008max   0.3max   0.08


Mechanical properties under Т=20oС for grade   St6ps   ( Ст6пс )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Rolled stock, GOST 535-2005     590 295-31512-15   


    Brinell hardness for     St6ps   ( Ст6пс )   ,       HB 10 -1 = 197   MPa


Technological properties for grade   St6ps   ( Ст6пс )
  Weldability: limited weldability.
 Flakes : not predisposed
Temper brittleness: not predisposed


Physical properties for grade   St6ps   ( Ст6пс )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7850    


Equivalent steels for grade     St6ps   ( Ст6пс )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandCanadaEuropeanItalyBelgiumSpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaAustriaSwitzerlandInter
-DIN,WNrJIS AFNORBSHGEN UNINBNUNEGBSSBDSMSZPNSTASCSNONORMSNVISO
A572
A572Gr.65
1.0060
E335
Fe590-2
St60-2
St60-2G
SM570
A60-2
E335
4360-55C
4360-55E
55C
E335
Fe590-2FN
480WT
1.0060
E335
Fe60-2FN
Fe60-3FN
E335
Fe590
Fe60-2
FE590-2FN
A590-2
E355
Fe590-2FN
HRB335
1650
ASt6
E335
WSt6sp
E355
Fe590-2
MSt6
St6
OL60.1k
11600
St60F
St60-2
Fe590



Types of delivery of grade   St6ps   ( Ст6пс )
В20 - Classification, nomenclature and general norms
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  St6ps   ( Ст6пс ) - Normal quality structural carbon steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru