Characteristics for grade     KH27YU5T   ( Х27Ю5Т )



      Grade :     KH27YU5T   ( Х27Ю5Т )
      Classification :   Precision alloy with higt electric resistance
      Equivalent grades:     Is absent



Chemical composition in % for grade   KH27YU5T   ( Х27Ю5Т )
C Si Mn Ni S P Cr Ce TiAl Ba Ca -
max   0.05max   0.6max   0.3max   0.6max   0.015max   0.0226 - 28max   0.10.15 - 0.45 - 5.8max   0.5max   0.1 Са, Ce,Ba - расчет


Mechanical properties under Т=20oС for grade   KH27YU5T   ( Х27Ю5Т )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Band, GOST 12766.2-90     785   10    


    Brinell hardness for     KH27YU5T   ( Х27Ю5Т )   ,       GOST 12766.1-90 HB 10 -1 = 200 - 250   MPa


Technological properties for grade   KH27YU5T   ( Х27Ю5Т )
  Weldability: without limitations.
 Flakes : not predisposed
Temper brittleness: predisposed


Technological properties of the material   KH27YU5T   ( Х27Ю5Т ) .
        Melting temperature : 1510   °C


Physical properties for grade   KH27YU5T   ( Х27Ю5Т )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7190   1360
100   15     500 1365
200           1370
300           1375
400           1380
500           1400
600           1400
700           1410
800           1410
900           1420
T E 10- 5 a 10 6 l r C R 10 9



Types of delivery of grade   KH27YU5T   ( Х27Ю5Т )
В32 - Graded and shaped rolling
B34 - Ribbons
B73 - Steel Alloy Wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  KH27YU5T   ( Х27Ю5Т ) - Precision alloy with higt electric resistance: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru