Characteristics for grade     18Kh15N3M-Sh   ( 18Х15Н3М-Ш )



      Grade :   18Kh15N3M-Sh   ( 18Х15Н3М-Ш ) (   18Х15Н3М     ДИ1-Ш     ДИ1   )
      Classification :   Corrosion-resistant high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   18Kh15N3M-Sh   ( 18Х15Н3М-Ш )
C Si Mn Ni S P Cr Mo W Cu -
0.15 - 0.21max   0.6max   0.62.5 - 3max   0.015max   0.0314.5 - 16.50.3 - 0.5max   0.5max   0.25 Остаточная доля Сu до 0.25%


Mechanical properties under Т=20oС for grade   18Kh15N3M-Sh   ( 18Х15Н3М-Ш )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar     930 735 14 55880Guenching 1050oC,Cooling oil, Drawing 640 - 680oC,Cooling air,
Bar     1130 885 12 50690Guenching 1050oC,Cooling oil, Drawing 540 - 580oC,Cooling air,



Types of delivery of grade   18Kh15N3M-Sh   ( 18Х15Н3М-Ш )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  18Kh15N3M-Sh   ( 18Х15Н3М-Ш ) - Corrosion-resistant high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru