Grade : | ANV-300 ( АНВ-300 ) ( АНВ300 ) |
Classification : | High-temperature casting alloy |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | W | Ti | Al | B | - |
max 0.1 | max 0.5 | max 0.5 | 64.2 - 70.1 | max 0.01 | max 0.015 | 14 - 17 | 7 - 10 | 1.4 - 2 | 4.5 - 5.5 | max 0.1 | Ni - basis |
OCT 1 90127-85 | |
Test temperature | 850 ° С |
Acting stress | 250 MPa |
Time to fracture, hours | 60 |
B51 - Non-ferrous metals, including rare metals, and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |