Characteristics for grade     V3K   ( В3К )



      Grade :     V3K   ( В3К )
      Classification :   High-temperature casting alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   V3K   ( В3К )
Fe C Si Ni S Cr W Co -
max   21 - 1.32 - 2.75max   2max   0.0728 - 324 - 554.8 - 65 Co - basis
Comment: Co is a basis; the percentage of Co is given approximately.


Mechanical properties under Т=20oС for grade   V3K   ( В3К )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Mechanical properties not regimented



Types of delivery of grade   V3K   ( В3К )
B51 - Non-ferrous metals, including rare metals, and their alloys
B55 - Bars


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  V3K   ( В3К ) - High-temperature casting alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru