Chemical composition in % for grade   06Kh12N3D   ( 06Х12Н3Д )
C Si Mn Ni S P Cr Cu
max   0.06max   0.3max   0.62.8 - 3.2max   0.025max   0.0312 - 13.50.8 - 1.1


Mechanical properties under Т=20oС for grade   06Kh12N3D   ( 06Х12Н3Д )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Forging to 250   686 588 12 35580 


    Brinell hardness for     06Kh12N3D   ( 06Х12Н3Д )   ,     Forging HB = 207 - 293   MPa




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  06Kh12N3D   ( 06Х12Н3Д ) - Corrosion-resistant high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru