Characteristics for grade     08KH17N13M2T   ( 08Х17Н13М2Т )



      Grade :   08KH17N13M2T   ( 08Х17Н13М2Т ) (   0Х17Н13М2Т   )
      Substitute:   10Х17Н13М2Т
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   08KH17N13M2T   ( 08Х17Н13М2Т )
C Si Mn Ni S P Cr Mo Cu -
max   0.08max   0.8max   212 - 14max   0.02max   0.03516 - 182 - 3max   0.3 (5 С - 0.7) Ti, остальное Fe


Mechanical properties under Т=20oС for grade   08KH17N13M2T   ( 08Х17Н13М2Т )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75 Ø 60   490 196 40 50 Guenching 1050 - 1100oC,
Sheet trick, GOST 7350-77     510 196 40   Guenching 1030 - 1080oC,Cooling air,


Technological properties for grade   08KH17N13M2T   ( 08Х17Н13М2Т )
  Weldability: without limitations.


Physical properties for grade   08KH17N13M2T   ( 08Х17Н13М2Т )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       8000    


Equivalent steels for grade     08KH17N13M2T   ( 08Х17Н13М2Т )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenPoland
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSPN
316Ti
S31635
1.4573
X10CrNiMoTi18-12
X6CrNiMoTi17-12-2
SUS316Ti
Z6CNDT17.12
320S33
1.4571
X6CrNiMoTi17-12-2
X6CrNiMoTi17-13
F.3535
X6CrNiMoTi17-12-2
0Cr18Ni12Mo3Ti
1Cr18Ni12Mo2Ti
1Cr18Ni12Mo3Ti
2350
H17N13M2T



Types of delivery of grade   08KH17N13M2T   ( 08Х17Н13М2Т )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  08KH17N13M2T   ( 08Х17Н13М2Т ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru