Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Stainless steel

Characteristics for grade     10KH14АG15   ( 10Х14АГ15 )



      Grade :   10KH14АG15   ( 10Х14АГ15 ) (   Х14АГ5     ДИ-13   )
      Substitute:   12Х18Н9, 08Х18Н10, 12Х18Н9Т, 12Х18Н10Т
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:     Is absent



Chemical composition in % for grade   10KH14АG15   ( 10Х14АГ15 )
C Si Mn Ni S P Cr N Ti Cu
max   0.1max   0.814.5 - 16.5max   0.6max   0.03max   0.04513 - 150.15 - 0.25max   0.2max   0.3


Mechanical properties under Т=20oС for grade   10KH14АG15   ( 10Х14АГ15 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet thin, GOST 5582-75     740   45   Guenching 950 - 1100oC,Cooling water,


Technological properties for grade   10KH14АG15   ( 10Х14АГ15 )
  Weldability: without limitations.


Physical properties for grade   10KH14АG15   ( 10Х14АГ15 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.05     7900    
100   13.9        
200            
300            
400 1.79 19.4        
500            
600   21.8        
700            
800   22.5        
T E 10- 5 a 10 6 l r C R 10 9



Types of delivery of grade   10KH14АG15   ( 10Х14АГ15 )
B23 - Sheets and Strips
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  10KH14АG15   ( 10Х14АГ15 ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.