Characteristics for grade     32KH06L   ( 32Х06Л )



      Grade :     32KH06L   ( 32Х06Л )
      Classification :   Casting alloy steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   32KH06L   ( 32Х06Л )
C Si Mn S P Cr
0.25 - 0.350.2 - 0.40.4 - 0.9max   0.05max   0.050.5 - 0.8


Mechanical properties under Т=20oС for grade   32KH06L   ( 32Х06Л )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88 to 100   638 441 10 20491Guenching 890 - 910oC,Drawing 620 - 660oC,


Technological properties for grade   32KH06L   ( 32Х06Л )
  Weldability: limited weldability.
 Flakes : not predisposed
Temper brittleness: not predisposed


Technological properties of the material   32KH06L   ( 32Х06Л ) .
        Linear shrinkage : 1.8   %


Heat treatment of the material   32KH06L   ( 32Х06Л )
Hardening 890 - 910 ° C, Tempering 620 - 660 ° C


Physical properties for grade   32KH06L   ( 32Х06Л )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.16   50 7850   235
100 2.11 12.4 49   491 269
200 2.07 12.8 46   508 333
300 1.95 13.2 42   521 425
400 1.78 13.6 39   533 527
500 1.74 14 36   567 658
600 1.66 14.4 32   584 797
700 1.46 14.7 29   622 952
800 1.31 12 26   701 1109
900   12.7 27   684 1158
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     32KH06L   ( 32Х06Л )
Warning! Indicated both exact and nearest equivalents.
BulgariaPoland
BDSPN
30ChL
L30H



Types of delivery of grade   32KH06L   ( 32Х06Л )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  32KH06L   ( 32Х06Л ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru