Characteristics for grade     M1rE   ( М1рЕ )



      Grade :     M1rE   ( М1рЕ )
      Classification :   Copper
      Equivalent grades:     Is absent



Chemical composition in % for grade   M1rE   ( М1рЕ )
Fe Ni S P As PbZn OSb Bi Sn -
max   0.005max   0.002max   0.0050.002 - 0.012max   0.002max   0.005max   0.005max   0.01max   0.002max   0.001max   0.002 Cu+Ag min 99.9


Mechanical properties under Т=20oС for grade   M1rE   ( М1рЕ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
soft cold-rolled, GOST 1173-2006     200-260  42    
hard cold-rolled, GOST 1173-2006     290   6    


    Brinell hardness for     M1rE   ( М1рЕ )   ,     soft GOST 1173-2006 HB 10 -1 = 55   MPa
    Brinell hardness for     M1rE   ( М1рЕ )   ,     hard GOST 1173-2006 HB 10 -1 = 95   MPa



Types of delivery of grade   M1rE   ( М1рЕ )
В54 - Ribbons


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  M1rE   ( М1рЕ ) - Copper: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru