Characteristics for grade     45KKhNMVT   ( 45КХНМВТ )



      Grade :     45KKhNMVT   ( 45КХНМВТ )
      Classification :   Corrosion-resistant alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   45KKhNMVT   ( 45КХНМВТ )
Fe C Si Mn Ni S P Cr Mo W Co Ti
4 - 6max   0.05max   0.5max   115 - 25max   0.01max   0.01518 - 223 - 43 - 444 - 460.5 - 3.5


Mechanical properties under Т=20oС for grade   45KKhNMVT   ( 45КХНМВТ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Wire heat-treatment, GOST 51396-99     600 275 50    
Wire, GOST 51396-99     1000 830 18    
Wire cold-worked , GOST 51396-99     1310 1170 12    



Types of delivery of grade   45KKhNMVT   ( 45КХНМВТ )
B73 - Steel Alloy Wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  45KKhNMVT   ( 45КХНМВТ ) - Corrosion-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru