Grade : | TsAM10-5L ( ЦАМ10-5Л ) |
Classification : | Zinc antifriction alloys |
Equivalent grades: | Is absent |
Fe | Si | Al | Cu | Pb | Mg | Zn | Sn | Cd | Impurity |
max 0.15 | max 0.1 | 9 - 12 | 4 - 5.5 | max 0.03 | 0.03 - 0.06 | 81.8 - 86.62 | max 0.01 | max 0.02 | all 0.35 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
, GOST 21437-95 | 245 | 0.4 |
Brinell hardness for TsAM10-5L ( ЦАМ10-5Л ) , GOST 21437-95 | HB 10 -1 = 100 MPa |
Load | Speed | Load * Speed | Temperature |
MPa | m/s | MPa * m/s | Grade |
9.8 | 8 | 80 |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |