Characteristics for grade     EhI698MP   ( ЭИ698МП )



      Grade :   EhI698MP   ( ЭИ698МП ) (   ВЖ136     ХН66ВМТЮБ   )
      Classification :   Heat-resistant nickel alloy regranulate
      Equivalent grades:     Is absent



Chemical composition in % for grade   EhI698MP   ( ЭИ698МП )
Fe C Si Mn Ni S P Cr Ce Mo W V Nb TiAl Zr B Mg
max   1.5max   0.04max   0.45max   0.466.44 - 74.1max   0.007max   0.01515.5 - 17.5max   0.013.8 - 4.40.8 - 1.50.8 - 1.52.2 - 2.60.8 - 1.22 - 2.4max   0.005max   0.005max   0.03
Comment: Ni is a basis; the percentage of Ni is given approximately.




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  EhI698MP   ( ЭИ698МП ) - Heat-resistant nickel alloy regranulate: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru