Characteristics for grade     D16   ( Д16 )



      Grade :   D16   ( Д16 ) (   1160   )
      Classification :   Aluminium wrought alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   D16   ( Д16 )
Fe Si Mn Cr TiAl Cu Mg Zn Impurity -
max   0.5max   0.50.3 - 0.9max   0.1max   0.1590.9 - 94.73.8 - 4.91.2 - 1.8max   0.25other, each 0.05; all 0.15 Ti+Zr < 0.2
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   D16   ( Д16 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 18482-79     390-420255-27510-12   
Bar, GOST 21488-97     245 120 12    
Bar, GOST 21488-97 Ø 8 - 300   390-410275-2958-10  Hardening and ageing
Bar, GOST 51834-2001     450-470325-3458-10  Hardening and ageing
Bar, GOST 51834-2001     410 265 12   Hardening and ageing
Band annealed , GOST 13726-97     235   10    
Profile, GOST 8617-81 10 - 150   412 284 10   Quenching and artificial aging
Profile annealed , GOST 8617-81     245   12    
Plate , GOST 17232-99     345-420245-2753-7  Hardening and ageing


    Brinell hardness for     D16   ( Д16 )   (quenching, ageing) ,       HB 10 -1 = 105   MPa
    Brinell hardness for     D16   ( Д16 )   ,     annealed HB 10 -1 = 42   MPa


Physical properties for grade   D16   ( Д16 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.72     2770    
100   22.9 130   0.922  


Equivalent steels for grade     D16   ( Д16 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyPolandCzechiaAustriaSwitzerlandInter
-DIN,WNrJIS AFNORBSEN UNIPNCSNONORMSNVISO
2024
AA2024
AA2124
3.1355
AlCuMg2
2024
2024
A-U4GI
2024
ENAW-2024
ENAW-AlCu4Mg1
P-AlCu4.4MgMn
AICu4Mg2
424203
AICuMg2
Al4Cu1.2Mg
2024
AlCu4Mg1
AlCuMg1



Types of delivery of grade   D16   ( Д16 )
B52 - Graded and shaped rolling
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  D16   ( Д16 ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru