Chemical composition in % for grade   АMg3   ( АМг3 )
Fe Si Mn Cr TiAl Cu Mg Zn Impurity
max   0.50.5 - 0.80.3 - 0.6max   0.05max   0.193.8 - 96max   0.13.2 - 3.8max   0.2other, each 0.05; all 0.1
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   АMg3   ( АМг3 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 18482-79     180 70 15    
Bar, GOST 21488-97     175 80 13    
Band annealed , GOST 13726-97     185-19580-10015    
Band, GOST 13726-97     245 195 7    
Profile, GOST 8617-81     176 78 12    
Plate , GOST 17232-99     165-18559-6911-12   


    Brinell hardness for     АMg3   ( АМг3 )   ,       HB 10 -1 = 45   MPa


Technological properties for grade   АMg3   ( АМг3 )
  Weldability: without limitations.


Physical properties for grade   АMg3   ( АМг3 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.71     2660   49.6
100   23.5 151   880  


Equivalent steels for grade     АMg3   ( АМг3 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySwedenPolandCzechiaAustriaInter
-DIN,WNrJIS AFNORBSEN UNISSPNCSNONORMISO
A95154
AA5154
3.3535
AIMg2.7Mn
AlMg3
5154
5254
5154A
5454
AWAIMg3
ENAW-5754
ENAW-AlMg3
PAIMg3.5
AIMG3
AIMg3
424413
AIMGg3
AlMg3



Types of delivery of grade   АMg3   ( АМг3 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B52 - Graded and shaped rolling
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  АMg3   ( АМг3 ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru