Characteristics for grade     АMts   ( АМц )



      Grade :   АMts   ( АМц ) (   1400   )
      Classification :   Aluminium wrought alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   АMts   ( АМц )
Fe Si Mn Al CuZn Impurity
max   0.7max   0.61 - 1.596.35 - 990.05 - 0.2max   0.1other, each 0.05; all 0.15
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   АMts   ( АМц )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 18482-79     100   12    
Pipe annealed , GOST 18475-82     90-135  15    
Pipe cold-worked , GOST 18475-82     135        
Bar, GOST 21488-97     100   20    
Band, GOST 13726-97     100   10    
Profile, GOST 8617-81     98   16    
Plate , GOST 17232-99     110-120  12-15   


    Brinell hardness for     АMts   ( АМц )   (cold-worked) ,       HB 10 -1 = 55   MPa
    Brinell hardness for     АMts   ( АМц )   ,     annealed HB 10 -1 = 30   MPa


Technological properties for grade   АMts   ( АМц )
  Weldability: without limitations.


Physical properties for grade   АMts   ( АМц )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.71     2730   34.5
100   23.2 180   1090  
200   25        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     АMts   ( АМц )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySwedenPolandCzechiaAustriaInter
-DIN,WNrJIS AFNORBSEN UNISSPNCSNONORMISO
A93003
AA3003
3.0511
3.0515
AIMn1
AlMn
AlMn1Cu
3003
3103
A-M1
3103
AWAIMn1
ENAW-3003
ENAW-3103
ENAW-AlMn1
ENAW-AlMn1Cu
PAIMn1.2Cu
AIMn
AIMn1
424432
AIMn
AlMn1
AlMn1Cu



Types of delivery of grade   АMts   ( АМц )
B51 - Non-ferrous metals, including rare metals, and their alloys
B52 - Graded and shaped rolling
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  АMts   ( АМц ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru