Characteristics for grade     АK5M   ( АК5М )



      Grade :   АK5M   ( АК5М ) (   АЛ5   )
      Classification :   Aluminium casting alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   АK5M   ( АК5М )
Fe Si Mn Al Cu Be Mg Zn Sn Impurity -
max   1.54.5 - 5.5max   0.590.7 - 94.151 - 1.5max   0.10.35 - 0.6max   0.3max   0.01 all 1.7 Ti+Zr<0.15
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   АK5M   ( АК5М )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 1583-93     157-235  0.5-1   


    Brinell hardness for     АK5M   ( АК5М )   ,     Casting GOST 1583-93 HB 10 -1 = 65 - 70   MPa


Physical properties for grade   АK5M   ( АК5М )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.7     2680   46.2
100   23.1 163   838  


Equivalent steels for grade     АK5M   ( АК5М )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanEnglandChinaCzechiaInter
-DIN,WNrJIS BSGBCSNISO
305.0
355.0
A03550
G-AlSi5(Cu)
G-AlSi5Mg
GK-AlSi5Mgwa
G—AlSi5Cu
AC4A
AC4D
3L78
LM16
HZL105
ZAlSi5CulMg
ZL105
424380
AlSi5Cu1Mg



Types of delivery of grade   АK5M   ( АК5М )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  АK5M   ( АК5М ) - Aluminium casting alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru