Characteristics for grade     BrKHNb   ( БрХНб )

      Grade :     BrKHNb   ( БрХНб )
      Classification :   High-temperature bronzes
      Equivalent grades:     Is absent



Chemical composition in % for grade   BrKHNb   ( БрХНб )
Fe Si P Cr Nb Cu Pb Mg Zn
max   0.06max   0.05max   0.010.3 - 0.50.1 - 0.498.94 - 99.6max   0.005max   0.02max   0.015
Comment: Cu is a basis; the percentage of Cu is given approximately.


Technological properties of the material   BrKHNb   ( БрХНб ) .
        Forging temperature : 700 - 950   °C
        Annealing temperature : 650 - 700   °C


Physical properties for grade   BrKHNb   ( БрХНб )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.35 17.1 380     18.5


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrKHNb   ( БрХНб ) - High-temperature bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru