Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Lead

Characteristics for grade     BS6   ( БС6 )



      Grade :     BS6   ( БС6 )
      Classification :   Lead babbits
      Equivalent grades:     Is absent



Chemical composition in % for grade   BS6   ( БС6 )
FeAl Cu As PbZn Sb Bi Sn Cd
max   0.1max   0.0050.1 - 0.3max   0.0586.415 - 88.9max   0.015.5 - 6.5max   0.075.5 - 6.5max   0.05
Comment: Pb is a basis; the percentage of Pb is given approximately.


    Brinell hardness for     BS6   ( БС6 )   ,       GOST 1320-74 HB 10 -1 = 15 - 17   MPa


Limiting operating condition of the material   BS6   ( БС6 )
Load Speed Load * Speed Temperature
MPa m/s MPa * m/s Grade
15    70


Technological properties of the material   BS6   ( БС6 ) .
        Melting temperature : 280   °C


Physical properties for grade   BS6   ( БС6 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       10050    



Types of delivery of grade   BS6   ( БС6 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BS6   ( БС6 ) - Lead babbits: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru