Characteristics for grade     VT16   ( ВТ16 )



      Grade :     VT16   ( ВТ16 )
      Classification :   Titanium wrought alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   VT16   ( ВТ16 )
Fe C Si Mo V N TiAl Zr OH Impurity
max   0.25max   0.1max   0.154.5 - 5.54 - 5max   0.0584.85 - 89.71.8 - 3.8max   0.3max   0.15max   0.015 other 0.3
Comment: Ti is a basis; the percentage of Ti is given approximately.


Mechanical properties under Т=20oС for grade   VT16   ( ВТ16 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar heat-treatment     1030-1225  12 50  
Sheet thin     840-1250  12-22  Annealing
Sheet thin     1300-1400  5-6 500Hardening and ageing


    Brinell hardness for     VT16   ( ВТ16 )   (quenching, ageing) ,     Sheet thin HB 10 -1 = 302 - 415   MPa


Technological properties for grade   VT16   ( ВТ16 )
  Weldability: without limitations.


Physical properties for grade   VT16   ( ВТ16 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.1          



Types of delivery of grade   VT16   ( ВТ16 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  VT16   ( ВТ16 ) - Titanium wrought alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys