Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Titanium

Characteristics for grade     VT9   ( ВТ9 )



      Grade :     VT9   ( ВТ9 )
      Classification :   Titanium wrought alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   VT9   ( ВТ9 )
Fe C Si Mo N TiAl Zr OH Impurity
max   0.25max   0.10.2 - 0.352.8 - 3.8max   0.0586.15 - 89.95.8 - 71 - 2max   0.15max   0.015 other 0.3
Comment: Ti is a basis; the percentage of Ti is given approximately.


Mechanical properties under Т=20oС for grade   VT9   ( ВТ9 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 26492-85     930-980  6-715-16200-250Annealing
Bar, GOST 26492-85     980-1230  7-916-30300Annealing
Die     1100-1300  8-1425-45200-500Annealing


Physical properties for grade   VT9   ( ВТ9 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.18     4510    



Types of delivery of grade   VT9   ( ВТ9 )
B55 - Bars


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  VT9   ( ВТ9 ) - Titanium wrought alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys