Characteristics for grade     VT20   ( ВТ20 )



      Grade :     VT20   ( ВТ20 )
      Classification :   Titanium wrought alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   VT20   ( ВТ20 )
Fe C Si Mo V N TiAl Zr OH Impurity
max   0.25max   0.1max   0.150.5 - 20.8 - 2.5max   0.0585.15 - 91.45.5 - 71.5 - 2.5max   0.15max   0.015 other 0.3
Comment: Ti is a basis; the percentage of Ti is given approximately.


Mechanical properties under Т=20oС for grade   VT20   ( ВТ20 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet annealed , GOST 22178-76     930-980  6-12  Annealing
Bar, GOST 26492-85     885   7-820250-300Annealing
Bar, GOST 26492-85     885-1130  8-1020-25300-400Annealing
Plate , GOST 23755-79 11 - 100   880-1130  5-610-12300Annealing


    Brinell hardness for     VT20   ( ВТ20 )   ,       HB 10 -1 = 255 - 341   MPa


Technological properties for grade   VT20   ( ВТ20 )
  Weldability: without limitations.


Physical properties for grade   VT20   ( ВТ20 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.12   8 4450   1110
100   8.3 8.8      
200   8.3 10.2   0.587  
300   9 10.9   0.628  
400   9.2 12.2   0.67  
500   9.3 13.8   0.712  
600   9.5 15.1      
T E 10- 5 a 10 6 l r C R 10 9



Types of delivery of grade   VT20   ( ВТ20 )
B53 - Sheets and Strips
B55 - Bars


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  VT20   ( ВТ20 ) - Titanium wrought alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru