Grade : | VT1-00 ( ВТ1-00 ) |
Classification : | Titanium |
Equivalent grades: | Go here |
Fe | C | Si | N | Ti | O | H | Impurity |
max 0.15 | max 0.05 | max 0.08 | max 0.04 | 99.58 - 99.9 | max 0.1 | max 0.008 | other 0.1 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet annealed , GOST 22178-76 | 295 | 20-30 | ||||||
Pipe, GOST 24890-81 | 294-441 | 20 | ||||||
Bar, GOST 26492-85 | 265-440 | 24-25 | 42-55 | 600-1200 | Annealing | |||
Bar annealed , GOST 26492-85 | 265-295 | 20 | 40-50 | 600-1000 | ||||
Plate , GOST 23755-79 | 11 - 150 | 295-490 | 11-14 | 25-28 |
Brinell hardness for VT1-00 ( ВТ1-00 ) , | HB 10 -1 = 116 - 143 MPa |
Weldability: | without limitations. |
Melting temperature : | 1668 °C |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 1.12 | 18.85 | 4505 | |||
100 | 8.2 | 540 |
USA | Germany | Japan | France | England | |||||||
- | DIN,WNr | JIS | AFNOR | BS | |||||||
|
|
|
|
|
B53 - Sheets and Strips |
B55 - Bars |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
Weldability : | |
without limitations | - welding is done without heating and subsequent heat treeting |
limited weldability | - welding is possible under heating up to 100-120 grade and subsequent heat treeting |
hard weldability | - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing |