Characteristics for grade     NMts5   ( НМц5 )



      Grade :     NMts5   ( НМц5 )
      Classification :   Nickel alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   NMts5   ( НМц5 )
Ni+Co Fe C Si Mn S P Cu As Pb Mg Sb Bi Impurity
92.6 - 95.4max   0.65max   0.15max   0.34.6 - 5.4max   0.015max   0.02max   0.2max   0.03max   0.002max   0.1max   0.002max   0.002 all 2
Comment: Ni+Co is a basis; the percentage of Ni+Co is given approximately.


Mechanical properties under Т=20oС for grade   NMts5   ( НМц5 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Wire, GOST 1049-74     740   18    
Wire, GOST 1049-74     740-980       
soft     500-550  42.5    
hard     950-1050  4    


Technological properties of the material   NMts5   ( НМц5 ) .
        Melting temperature : 1410   °C
        Forging temperature : 1200 - 900   °C
        Annealing temperature : 800 - 900   °C


Physical properties for grade   NMts5   ( НМц5 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.1     8760   200
100   13.7        


Equivalent steels for grade     NMts5   ( НМц5 )
Warning! Indicated both exact and nearest equivalents.
Germany
DIN,WNr
2.4116
NiMn5



Types of delivery of grade   NMts5   ( НМц5 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  NMts5   ( НМц5 ) - Nickel alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru