Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Nickel

Characteristics for grade     NPАN   ( НПАН )



      Grade :     NPАN   ( НПАН )
      Classification :   Semis nickel
      Equivalent grades:     Is absent



Chemical composition in % for grade   NPАN   ( НПАН )
Ni+Co Fe Si Mn S Cu OImpurity
min   99.4max   0.1max   0.03max   0.050.002 - 0.010.01 - 0.10.03 - 0.3 all 0.6


Technological properties of the material   NPАN   ( НПАН ) .
        Melting temperature : 1455   °C
        Forging temperature : 1140 - 1250   °C
        Annealing temperature : 700 - 800   °C
        Casting temperature : 1550 - 1650   °C
        Linear shrinkage : 1   %



Types of delivery of grade   NPАN   ( НПАН )
B51 - Non-ferrous metals, including rare metals, and their alloys
B53 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  NPАN   ( НПАН ) - Semis nickel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru