Characteristics for grade     BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф )



      Grade :     BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф )
      Classification :   Tin-free foundary bronzes
      Equivalent grades:     Is absent



Chemical composition in % for grade   BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф )
Fe Si Ni PAl Cu As PbZn Sb Bi Sn Impurity
max   0.3max   0.023 - 40.15 - 0.3max   0.0264.8 - 72.85max   0.118 - 223 - 43 - 4max   0.025max   0.5 all 0.9
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 493-79     157   2    


    Brinell hardness for     BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф )   ,     cast in a metal mould GOST 493 HB 10 -1 = 65   MPa


Technological properties of the material   BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф ) .
        Linear shrinkage : 1.25   %


Physical properties for grade   BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.735 17.4 54.4 9100    




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrSu3N3TS3S20F   ( БрСу3Н3Ц3С20Ф ) - Tin-free foundary bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru