Characteristics for grade     BrOF6.5-0.15   ( БрОФ6.5-0.15 )



      Grade :     BrOF6.5-0.15   ( БрОФ6.5-0.15 )
      Classification :   Wrought tin bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrOF6.5-0.15   ( БрОФ6.5-0.15 )
Fe Si Ni PAl Cu PbZn Sb Bi Sn Impurity
max   0.05max   0.002max   0.20.1 - 0.25max   0.00292.28 - 93.8max   0.02max   0.3max   0.002max   0.0026 - 7 all 0.1
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrOF6.5-0.15   ( БрОФ6.5-0.15 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 10025-78     350   40    
Bar, GOST 10025-78     470   12    
Bar, GOST 10025-78     340   55    
Strip, GOST 1789-70     290 130 35-38   
Strip, GOST 1789-70     570-740540-7103-5   


    Brinell hardness for     BrOF6.5-0.15   ( БрОФ6.5-0.15 )   ,     Bar GOST 10025-78 HB 10 -1 = 140 - 150   MPa
    Brinell hardness for     BrOF6.5-0.15   ( БрОФ6.5-0.15 )   ,     Bar GOST 10025-78 HB 10 -1 = 70   MPa
    Brinell hardness for     BrOF6.5-0.15   ( БрОФ6.5-0.15 )   ,     Bar GOST 10025-78 HB 10 -1 = 70   MPa


Friction coefficient of the material   BrOF6.5-0.15   ( БрОФ6.5-0.15 ) .
 Friction coefficient with oil : 0.01
 Friction coefficient without oil : 0.12


Technological properties of the material   BrOF6.5-0.15   ( БрОФ6.5-0.15 ) .
        Melting temperature : 995   °C
        Forging temperature : 700 - 800   °C
        Annealing temperature : 600 - 650   °C


Physical properties for grade   BrOF6.5-0.15   ( БрОФ6.5-0.15 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.12   71.4 8800   160
100   17.1        


Equivalent steels for grade     BrOF6.5-0.15   ( БрОФ6.5-0.15 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanSwedenPolandCzechiaAustriaInter
-DIN,WNrJIS AFNORBSEN SSPNCSNONORMISO
C51900
2.1020
CuSn6
C5191
CuSn6P
PB102
CuSn6
CW452K
CuSn6
CuSn6
423016
CuSn6
CuSn6



Types of delivery of grade   BrOF6.5-0.15   ( БрОФ6.5-0.15 )
В05 - Welding and cutting of metals., Soldering, riveting
B53 - Sheets and Strips
B55 - Bars


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrOF6.5-0.15   ( БрОФ6.5-0.15 ) - Wrought tin bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru