Characteristics for grade     LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )



      Grade :   LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 ) (   ЛАЖМц66-6-3-2   )
      Classification :   Cast cooper-zinc alloys
      Equivalent grades:   Go here



Chemical composition in % for grade   LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )
Fe Si Mn NiAl Cu PbZn Sb Sn Impurity
2 - 4max   0.31.5 - 3max   14 - 764 - 68max   0.716.2 - 28.5max   0.1max   0.7 all 1.8
Comment: Zn is a basis; the percentage of Zn is given approximately.


Mechanical properties under Т=20oС for grade   LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould, GOST 17711-93     705   7    
sand (mould) casting, GOST 17711-93     686   7    


    Brinell hardness for     LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )   ,     cast in a metal mould GOST 17711-93 HB 10 -1 = 165   MPa
    Brinell hardness for     LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )   ,     sand (mould) casting GOST 17711-93 HB 10 -1 = 160   MPa


Technological properties of the material   LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 ) .
        Melting temperature : 900   °C


Physical properties for grade   LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20   19.8 50.2 8500    


Equivalent steels for grade     LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEuropeanCzechia
-DIN,WNrJIS AFNOREN CSN
C86200
C86300
G-CuZn25Al5
H5102/class3
H5102/class4
HBsC4
CuZn19AI6Y20
CC762S
CuZn25Al5Mn4Fe3-C
423311



Types of delivery of grade   LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  LTS23А6ZH3Mts2   ( ЛЦ23А6Ж3Мц2 ) - Cast cooper-zinc alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru