Characteristics for grade     BrO5TS5S5   ( БрО5Ц5С5 )



      Grade :   BrO5TS5S5   ( БрО5Ц5С5 ) (   БрОЦС5-5-6   )
      Classification :   Tin foundry bronzes
      Equivalent grades:   Go here



Chemical composition in % for grade   BrO5TS5S5   ( БрО5Ц5С5 )
Fe Si PAl Cu PbZn Sb Sn Impurity
max   0.4max   0.05max   0.1max   0.0580.7 - 884 - 64 - 6max   0.54 - 6 all 1.3
Comment: Cu is a basis; the percentage of Cu is given approximately.


Mechanical properties under Т=20oС for grade   BrO5TS5S5   ( БрО5Ц5С5 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 24301-93     200-240  15-20   
cast in a metal mould, GOST 613-79     176   4   Without heat treatment
sand (mould) casting, GOST 613-79     147   6   Without heat treatment


    Brinell hardness for     BrO5TS5S5   ( БрО5Ц5С5 )   (without heat treatment) ,       GOST 613-79 HB 10 -1 = 60   MPa
    Brinell hardness for     BrO5TS5S5   ( БрО5Ц5С5 )   ,     Bar GOST 24301-93 HB 10 -1 = 65 - 70   MPa


Friction coefficient of the material   BrO5TS5S5   ( БрО5Ц5С5 ) .
 Friction coefficient with oil : 0.016
 Friction coefficient without oil : 0.26


Technological properties of the material   BrO5TS5S5   ( БрО5Ц5С5 ) .
        Casting temperature : 1250 - 1300   °C
        Linear shrinkage : 1.5   %


Physical properties for grade   BrO5TS5S5   ( БрО5Ц5С5 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.926 19.1   8800 393  


Equivalent steels for grade     BrO5TS5S5   ( БрО5Ц5С5 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySwedenPolandCzechia
-DIN,WNrJIS AFNORBSEN UNISSPNCSN
C83600
C83800
2.1097
GCuSn5Zn5Pb
Rg5
BC6
H5111/class6
H5111/class6C
CuSn5Pb5Zn5
LG2
CuSn5Zn5Pb5-C
GCuSn5Zn5Pb5
CuSn5Pb5Zn5
CuSn5Zn5Pb5
423135



Types of delivery of grade   BrO5TS5S5   ( БрО5Ц5С5 )
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  BrO5TS5S5   ( БрО5Ц5С5 ) - Tin foundry bronzes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru